Ma muli o ka pipiʻi nui o ka carbide cemented, he mea nui ka hoʻohana pono ʻana i nā drill carbide cemented e hoʻohana pono i ia mau mea e hōʻemi i nā kumukūʻai hana. ʻO ka hoʻohana pono ʻana i nā carbide drills ka mea nui i kēia mau ʻano:
micro drill
1. E koho i ka mīkini pono
ʻO nā pahu hoʻoheheʻe Carbidehiki ke hoʻohana ʻia i nā mīkini mīkini CNC, nā kikowaena mīkini a me nā mea mīkini ʻē aʻe me ka mana kiʻekiʻe a me ka rigidity maikaʻi, a pono e hōʻoia i ka holo ʻana o ka tip TIR <0.02. Eia nō naʻe, ma muli o ka haʻahaʻa haʻahaʻa a me ka maikaʻi ʻole o ka spindle pololei o nā mea mīkini e like me nā radial drills a me nā mīkini wili honua, he maʻalahi ke kumu o ka hāʻule mua ʻana o nā drill carbide, pono e pale ʻia e like me ka hiki.
2. E koho i ka lima pono
Hiki ke hoʻohana ʻia nā puna puna, nā ʻaoʻao kaomi ʻaoʻao, nā mea paʻa hydraulic, nā mea paʻa hoʻonui wela, a me nā mea ʻē aʻe, akā ma muli o ka lawa ʻole o ka ikaika hoʻopaʻa ʻana o ka puʻupuʻu hoʻololi wikiwiki, e paheʻe ka drill bit, no laila pono e pale ʻia.
3. hooluolu pololei
(1) Pono ka hoʻoluʻu waho e hoʻolohe i ka hui ʻana o nā kuhikuhi hoʻoluʻu, e hana i kahi hoʻonohonoho alapiʻi luna a me lalo, a hoʻemi i ke kihi me ka mea hana e like me ka hiki.
(2) Pono e hoʻolohe ka mea hoʻoluʻu o loko i ke kaomi a me ke kahe, a pono e pale i ka leakage o ka mea hoʻomaha mai ka hopena i ka hopena hoʻomaha.
4. ʻO ke kaʻina hana wili pololei
(1) Ke ʻae ʻia ka wili ʻana o ka ʻili o ka wili ʻana ma> 8-10 °. Ke <8-10°, pono e hoemi i ka ai i ka 1/2-1/3 o ka ma'amau;
(2) Ke hoʻemi ʻia ka ʻaoʻao o ka wili ʻana o ka ʻili he> 5 °, pono e hoʻemi ʻia ka hānai i 1 / 2-1 / 3 o ka mea maʻamau;
(3) I ka wili ʻana i nā lua keʻa (nā puka orthogonal a i ʻole nā puka oblique), pono e hoʻemi ʻia ka hānai i 1/2-1/3 o ka mea maʻamau;
(4) ʻAʻole pāpā ʻia nā ʻohe 2 no ka reaming.